Stainless Steel Bar
347 stainless steel is made of a high-temperature oxidation-resistant stainless steel material mainly consisting of chromium, nickel and titanium. It can be used at high temperatures and resists corrosion and oxidation effectively.
Big fire special steel, high strength steel plate, steel industry supply and demand, steel suppliers
347 is a stable austenitic chromium steel, containing niobium, which can eliminate carbide precipitation, thereby eliminating corrosion during the year. 347 is stabilized by the addition of chromium and tantalum, and provides higher creep and stress rupture properties than alloys 304 and 304L, which can also be used for sensitization and exposure to corrosion problems during the year. The addition of niobium also makes the 347 alloy have excellent corrosion resistance, even better than the 321 alloy.
Product Parameters
Product Name 347 Stainless Steel Bar Type Steel Bar Outer Diameter Round Bar 4mm-500mm Hexagon Bar 18mm-57mm (11/16″ to 2-3/4″) Square Bar 18mm-47mm (11/16″ to 1-3/4″) Flat Steel 1/2 "to 10", Thickness: 2mm-150mm, Can provide customized Length 1-6 meters, Length can be customized Standard ASTM, AISI, JIS, GB, DIN, EN, etc. Surface Black, Bright Polished, Rough Turning, Mattness Surface Treatment, No. 4. BA, etc. Scope of Application Stainless steel bars are used in a variety of industries such as shipbuilding, Defense, Automotive, Textiles, Paper and pulp, Manufacturing, Cement, Heavy earthmoving equipment and construction, etc.
Chemical Composition
C Si Mn Cr Ni S P ≤ 0.08 ≤ 0.75 ≤ 2.0 18.0~20.0 9.0~13.0 ≤ 0.03 ≤ 0.04
Mechanical Properties
Tensile Strength Kb (MPa) Yield Strength σ0.2 (MPa) Elongation D5 (%) Hardness ≥515 ≥205 ≥ 40 ≤ 201HB;≤ 95HRB
Physical Performance
Density(g/cm³) Modulus of Elasticity(Gpa) Coefficient of Thermal Expansion(10-6/°C) Coefficient of Thermal Conductivity(W/m*K) Resistivity(ΜΩ. cm) 7.97 193 16.0 16.3 72